0% penetration.
Incorrect filler?
No clue
Looks more like that to me. Maybe magnesium filler on aluminum?
Was it downhill on very very low voltage and dirty material? I can’t imagine another way of doing that
I have no idea who did it, it was brought to my shop to “fix”
Wtf were the settings
No clue, it was brought to me to “fix”
That’s good. No grinding out bad welds
True, half of the welds just fell off lol
Thats so bad it looks like it took talent
Had a student that was learning how to GTAW stainless weld on carbon pipe and accidentally grabbed an aluminum rod instead of stainless. Asked for my help because he was struggling and I immediately saw the rod before even seeing the weld. He had, somehow, been able to weld a bead about 2” long.
I knew that it was technically possible (have had experience with what we call “pot metal”) but had never seen pure aluminum to pure carbon steel. I spent about an hour trying to duplicate it and could not. I still don’t know how he made it happen!
It’s amazing what one can accomplish when one doesn’t know what one can’t do.
Oh that was me when I used a a plasma cutter for the first time. Instructor accidentally set it to gouge when they were correcting the setting, and I still managed to cut through and get it clean on one side despite it being gouge. The other side of the metal looked like shit though.
Master oogway
Master Garfield.
Beginners luck
I had a coworker GMAW aluminum with 70s thinking that it was steel. It worked pretty well all things considered in that the pieces didn’t just snap apart
I like doing it like this, that way I can take all my welds home with me at the end of the day to show my family.
That’s not what yo mama said
I’m a rank amateur welder and I wouldn’t know how to do that even if I wanted to .
Just the tip
We had a mechanic weld on skid proof ladder rungs onto an existing ladder. We peeled his welds off just like in the photo. My buddy taped one of them on the front of his tool box as a mark of shame. He ended up getting fired for pencil whipping work orders not too long after this occurred.
This is…not…possible…is it?
I weld pallets together with a nail gun. Guys im not trolling, we had a really REALLY hill Billy fella come in a tell us that, he was damn serious, the boss gave him a position, ( not welder) and he’s been with us 11 years lol. Definately saw something in the guy
Looks like it has slag from gauging in it.
Its aluminum
You sure it wasn’t magnesium?
Just like high school huh?
Impressive it must have taken sheer skill to mess up this badly
Buddy definitely grabbed the wrong spool
Reminds me of that time when I was practicing MIG Aluminium and I grabbed a practice piece from a pile, starting laying beads, and the alumimium was flying off the plate, and shoorting accross the table. I was puzzled, checked the settings, the gas, tried again etc… Until I realised I had taken a plate of stainless from the wrong pile. Never been a morning person.
That’s ok, it happens to the best of us, even to young men. You just probably just need to de-stress.
Spool gun and run
thats just 3d printing
That’s what she said….with a large frown.
What she said
It’s like one of those rubber stickers 🤣
Amazing mate
Happened to me like few months back…They weren’t normal electrodes for welding..Some hard for protecting equipement…I yust pried them off with crowbar
I experienced similar a few years back. I bought a trailer that needed to be modded to accommodate my boat. There were those princess auto tail light housings welded on to the frame and they looked plenty fine to use as a jacking point on an unloaded trailer (I thought). As I raised the jack, the housing simply peeled off, and it was welded top and sides. Based on the welds on the rest of the trailer there was no way the same person did those housings. I only TIG so I’m stupid when it comes to MIG and stick, but I’m guessing you can just deposit metal right on top with no penetration if you get the settings just right?
0% penetration? Sounds like my sex life….